My report on the new Cryo Strings from Live Steel Strings.
I don't make a living selling Steel Guitar Strings but it has been great fun developing something that enhances the enjoyment we all have when playing our Steel Guitars.
The New Cryo Strings have Better Tone, Stay in Tune better, Last Longer, Have more Sustain than any string that has ever been made.
I have never heard anything that is in the same Zip Code as the new Cryo Strings.
Now here is a Bold statement:
If you find this not to be true, send them back to me in 30 days and I will refund your money.
Sid Hudson

I don't make a living selling Steel Guitar Strings but it has been great fun developing something that enhances the enjoyment we all have when playing our Steel Guitars.
The New Cryo Strings have Better Tone, Stay in Tune better, Last Longer, Have more Sustain than any string that has ever been made.
I have never heard anything that is in the same Zip Code as the new Cryo Strings.
Now here is a Bold statement:
If you find this not to be true, send them back to me in 30 days and I will refund your money.
Sid Hudson

- Rick Aiello
- Posts: 4855
- Joined: 11 Sep 2000 12:01 am
- Location: Berryville, VA USA
- Contact:
I got mine in the mail yesterday ... They are magnificent !!
I play a six string frypan ... And use unconventional gauges ... So I bought both available sets to mix/match ...
0.017
0.018
0.020p
0.022p
0.034
0.038
When I was making horseshoe magnets for Jason Lollar ... After heat treating, machining and finishing the alloy horseshoes ... I sent them for cryo treatment.
It was expensive, but worth it ... Drastically increased the martensite to austenite ratio ... Which increased the alloy's remanence (Br) ...
Big fan of cryo ...
I play a six string frypan ... And use unconventional gauges ... So I bought both available sets to mix/match ...
0.017
0.018
0.020p
0.022p
0.034
0.038
When I was making horseshoe magnets for Jason Lollar ... After heat treating, machining and finishing the alloy horseshoes ... I sent them for cryo treatment.
It was expensive, but worth it ... Drastically increased the martensite to austenite ratio ... Which increased the alloy's remanence (Br) ...
Big fan of cryo ...